The letters
"TDK" where written by applying a voltage on the epitaxial thin film
relative to the probe, then imaged in DC-EFM mode. The smallest polarized
bit size is 25nm which suggests the possibility of a recording density
of >400 Tbit/in2.
Image
courtesy of Yasuko Ichikawa, Toyo Corporation, Japan